Optical Spectroscopy-Based Multiple Defects Detection for GTAW
摘要
The welding utilized 5A06 aluminum alloy, measuring 300 mm in length, 50 mm in width, and 4 mm in thickness. Employed in the experiment was a pulse square wave alternating current for welding. The peak period and base period were set at 0.5 s each, with a peak current of 240 A and a base current of 50 A.