AM and Machining: Strategy
摘要
A product needs to be fabricated with the help of powder bed fusion (PBF) and machining. If the whole product is made by PBF, it is expensive and takes considerable time. If it is made by machining, a lot of materials need to be removed to make thin features. These features have a propensity to break during machining, and if any breaks occur, machining needs to be restarted. What should be the strategy to make it?