<p>Enhancing the performance and sustainability of concrete is critical in modern construction, and in-situ carbonation offers a promising approach by introducing CO<sub>2</sub> directly during mixing. This study investigates the influence of CO<sub>2</sub> dosage on the workability, durability, and strength of concrete with varying water-to-binder ratios. Gaseous CO<sub>2</sub> was injected during mixing, leading to the immediate formation of amorphous calcium carbonate and a noticeable reduction in slump within 10&#xa0;min. Experimental results showed that CO<sub>2</sub> addition improved pore structure and chloride resistance, with reductions of up to 18% in total charge and 13% in migration coefficient. However, a decrease in 28-day compressive strength was observed, varying with mix design. These findings highlight the importance of carefully balancing CO<sub>2</sub> dosage and water-to-binder ratio to enhance durability without compromising long-term strength.</p>

错误:搜索内容不能为空,请输入英文关键词
错误:关键词超出字数限制,请精简
高级检索

Effects of Water-to-Binder Ratios on the Workability, Durability and Strength Development of In-Situ Carbonated Concrete

  • Melaku N. Seifu,
  • Jemal Kedir Adem,
  • Hammad R. Khalid,
  • G. M. Kim,
  • Solmoi Park

摘要

Enhancing the performance and sustainability of concrete is critical in modern construction, and in-situ carbonation offers a promising approach by introducing CO2 directly during mixing. This study investigates the influence of CO2 dosage on the workability, durability, and strength of concrete with varying water-to-binder ratios. Gaseous CO2 was injected during mixing, leading to the immediate formation of amorphous calcium carbonate and a noticeable reduction in slump within 10 min. Experimental results showed that CO2 addition improved pore structure and chloride resistance, with reductions of up to 18% in total charge and 13% in migration coefficient. However, a decrease in 28-day compressive strength was observed, varying with mix design. These findings highlight the importance of carefully balancing CO2 dosage and water-to-binder ratio to enhance durability without compromising long-term strength.