Electrical Resistivity, Seebeck Coefficient, and Hall Coefficient of Pure Thallium at 100−550 K
摘要
Abstract
Electrical resistivity, Seebeck coefficient and Hall coefficient of pure thallium were measured at temperatures from 100 to 550 K, i.e. almost to the melting temperature of this metal. The history of the experiemental investigations of the transport properties of Tl is shortly reviewed. This is a first publication of the experimental data on the Seebeck coefficient and the Hall coefficient of Tl in such a broad temperature range.