<p>This study explores a hydrogen-assisted mineral phase transformation process with synergistic desulfurization for the efficient recovery of iron from the high-pressure acid leach (HPAL) tailings of laterite nickel ore. HPAL tailings containing 51.50wt% iron and 2.09wt% sulfur present environmental challenges due to their sulfur content. Pre-treatment at 950°C for 15 min successfully reduced the sulfur content to 0.295wt% and increased the iron grade to 57.66wt%. Further hydrogen-assisted mineral phase transformation at 520°C for 30 min, using 40vol% hydrogen and a gas flow rate of 600 mL·min<sup>−1</sup>, resulted in a product with an iron grade of 61.00wt% and 90.11% iron recovery. The overall desulfurization rate reached 85.83% when wet scrubbing and limestone were used to capture the sulfur. This study demonstrates the efficiency of this hydrogen-assisted process for sustainable iron recovery and sulfur removal from laterite nickel ore tailings, with potential for industrial applications.</p>

错误:搜索内容不能为空,请输入英文关键词
错误:关键词超出字数限制,请精简
高级检索

Hydrogen-assisted mineral phase transformation for iron recovery and sulfur removal from laterite nickel ore tailings

  • Na Zhao,
  • Yuchao Qiu,
  • Sainan Qi,
  • Mengyu He,
  • Qianwen Li,
  • Yongsheng Sun

摘要

This study explores a hydrogen-assisted mineral phase transformation process with synergistic desulfurization for the efficient recovery of iron from the high-pressure acid leach (HPAL) tailings of laterite nickel ore. HPAL tailings containing 51.50wt% iron and 2.09wt% sulfur present environmental challenges due to their sulfur content. Pre-treatment at 950°C for 15 min successfully reduced the sulfur content to 0.295wt% and increased the iron grade to 57.66wt%. Further hydrogen-assisted mineral phase transformation at 520°C for 30 min, using 40vol% hydrogen and a gas flow rate of 600 mL·min−1, resulted in a product with an iron grade of 61.00wt% and 90.11% iron recovery. The overall desulfurization rate reached 85.83% when wet scrubbing and limestone were used to capture the sulfur. This study demonstrates the efficiency of this hydrogen-assisted process for sustainable iron recovery and sulfur removal from laterite nickel ore tailings, with potential for industrial applications.