<p>Mechanical properties and features of fracture microrelief in welded joints of 1201 aluminum alloy, obtained by constricted arc welding at different speeds (24–120 m/h), were studied. The joint ductility is the highest when welding at a&#xa0;speed of 24 m/h, and energy-intensive pit microrelief and deformation ridges are formed on the fracture surface. The strength of joints in this case slightly decreases, but their ductility increases.</p>

错误:搜索内容不能为空,请输入英文关键词
错误:关键词超出字数限制,请精简
高级检索

The influence of constricted arc welding speed on the fracture of 1201 aluminum alloy joints

  • T. M. Labur

摘要

Mechanical properties and features of fracture microrelief in welded joints of 1201 aluminum alloy, obtained by constricted arc welding at different speeds (24–120 m/h), were studied. The joint ductility is the highest when welding at a speed of 24 m/h, and energy-intensive pit microrelief and deformation ridges are formed on the fracture surface. The strength of joints in this case slightly decreases, but their ductility increases.